Was awful compared with the SA stainless....
http://img.tapatalk.com/d/14/05/02/ybevu6es.jpg
Sent from my SGH-T889 using Tapatalk
Printable View
Was awful compared with the SA stainless....
http://img.tapatalk.com/d/14/05/02/ybevu6es.jpg
Sent from my SGH-T889 using Tapatalk
Pardon my ignorance, but what was awful? The frame itself, or something about welding carbon steel?
As Charles Barkley would say: "It's just turrible."
I think you should send that abomination to me forthwith and I will struggle with the burden of owning it ;)
JK, that work still looks amazing. Let's face it, at least it wasn't worked over with a ball peen hammer. I seem to recall a post about welding up a frame that got the "1960's garage gunsmith" treatment like that.
This frame and filler combo sputtrted and splattered significantly.
The SA was like perfectly done artisan bacon. This was more like tactical canned bacon. Best analogy I can come up with.
Sent from my SGH-T889 using Tapatalk